Sm₂co₁₇ · documented grade
XGS 25-T500
High-temperature SmCo. Published property values at 20 °C and 500 °C; application suitability requires engineering confirmation.
Material data
Published magnetic properties
Values apply at the stated test temperature. Scroll wide tables horizontally.Swipe the table sideways for all properties. The grade stays visible; each row has its own test temperature.
| Grade | Test temperature °C | Remanence, Br T | Intrinsic coercivity, Hcj kOe | Energy product, (BH)max MGOe | Published max. temperature °C |
|---|---|---|---|---|---|
| XGS 25-T500 | 20 | 0.95–1.03 | ≥25 | 22–25 | 500 |
| XGS 25-T500 | 500 | 0.65–0.80 | 6.6–9.0 | 10–13 | 500 |
Published maximum temperature is not a universal operating guarantee. Geometry, reverse field, load line and exposure conditions determine suitability. Br = remanence; Hcj = intrinsic coercivity, not Hcb.
Specification before selection
Confirm temperature, geometry, reverse field and acceptance criteria before selecting XGS 25-T500 for your system.
The values above reproduce the supplied grade table. They are not extrapolated curves or a guaranteed operating envelope.